NECESSITY OF RUSSIAN NANOINDENTATION STANDARD BASE DEVELOPMENT

Edward Aslanyan, Peter Krasowski
  • Abstract:
    Over the past years a large number of papers have been published on the application of the nanoindentation method. These works describe various aspects of the nanoindentation method and provide a detailed overview of the characteristics of different hardware and software tools implementing this method. However, measurements taken under the same conditions and on the seemingly same samples often provide a significant discrepancy in the results on different instruments functioning according to the same principle. This paper discusses the issues of metrological support for the nanoindentation method in Russia.
  • Keywords:
    nanoindentation method, Martens hardness, primary standard machine
  • DOI:
    _unreg_tc5-2010.015

Event details:

[EVENTDETAILS]
  • IMEKO TC:
    TC5
  • Event name:
    HARDMEKO 2010
  • Title:
    11th HARDMEKO Conference: HARDMEKO 2010 (together with 21st TC3 Conference on Measurement of Force, Mass and Torque and 2nd TC22 Meeting on Vibration Measurement)
  • Place:
    Pattaya, THAILAND
  • Time:
    21 November 2010 - 25 November 2010